Civil & Structural

Concrete Grades: Cube vs Cylinder

European grading names concrete by two characteristic compressive strengths in MPa: cylinder first, then cube.

Reading the grade

  • C30/37: 30 MPa on 150 × 300 mm cylinders, 37 MPa on 150 mm cubes.
  • Cubes give higher results because the platen restraint is greater on a squat specimen.
  • Gulf specifications and testing labs usually work in cube strength, so confirm which value a drawing means.

Hot weather concreting

  • High temperature speeds setting, increases water demand and causes plastic shrinkage cracks.
  • Typical controls: chilled water or ice, night pours, retarders, wind breaks and immediate curing.
  • Many Gulf specifications cap concrete temperature at placing at around 32 °C. Check your project specification.

Common grades

GradeTypical use
C20/25Blinding (lower), non-structural slabs
C30/37General slabs, beams and columns
C40/50Foundations in aggressive soils, post-tensioned slabs
C50/60+High-rise columns, precast
Good to knowCubes are normally tested at 7 and 28 days. The 28-day result decides compliance.